17-4 H1075 Stainless Steel

 

Stainless steel 17-4 H1075 has been heat treated at a temperature between 1065° F and 1085° F for 225-255 minutes. After treating the steel at a temperature of 1075° or higher, it will become softer than in the annealed form.

Specifications:

Condition A material heated 4 hours at specific temperature, and air cooled.

Applications:

Pump shafts, oil patch, aerospace.